Choosing ceramic floor tiles

Colour and size are the first things anyone notices about a floor tile. How the floor wears, and how it feels underfoot when it is wet, depends on details in the tile's data sheet. This page explains those details, and what to check before the first tile goes down.

Green glazed ceramic floor tiles laid in herringbone
Photo: Lishuilynn, CC BY-SA 4.0, via Wikimedia Commons (resized)

The standards behind the box

The main British and European standard for ceramic tiles is BS EN 14411. It covers how tiles are defined, classified and marked. A separate test, BS EN ISO 10545-7, measures how well the surface of a glazed tile stands up to wear.

The British code of practice for tiled floors is BS 5385-3. It covers the design and installation of ceramic floor tiling. The Tile Association, the trade body for tiling, lists these standards on its website. Ask the seller for the tile's data sheet, and check it shows results for the room you have in mind.

Slip resistance

A slip rating tells you how a floor is likely to behave when it is wet. The Health and Safety Executive (HSE) uses the pendulum test as its standard method. It gives a pendulum test value, or PTV. HSE treats a PTV of 36 or more as low slip potential, 25 to 35 as moderate, and 24 or less as high.

Many European flooring makers give an R rating instead, from R9 to R13, taken from a German ramp test. HSE warns that floors rated R9, and in some cases R10, will be slippery when wet or greasy. It also points out that each R class covers a wide range of slipperiness. For areas where people go barefoot, testers use a different rubber slider on the pendulum.

At work, the law requires floors to be suitable for the work done on them and kept in good condition.

Getting the floor ready

The Tile Association says a cement and sand screed should be kept covered to cure for at least 7 days. It should then dry out for a further 2 weeks before tiling.

On a timber floor, the association says a plywood overlay should be at least 15mm thick. The boards are screwed to the joists and noggins at 300mm centres. A primer helps the adhesive bond where the surface needs one, and PVA should never be used as a primer.

Joints and grout

Under BS 5385-3, the joints between floor tiles should be at least 3mm wide. Grout for tiles has its own standard, BS EN 13888. The Tile Association warns that cleaning grout off too early can leave the colour patchy. It can also leave a weak, dusty surface.

Old floors and asbestos

An older floor may need lifting before new tiles go down. Asbestos was widely used in homes until it was banned in 1999. HSE says it was added to some PVC and thermoplastic floor tiles, and to the bitumen adhesive used to stick tiles down. Old asbestos floor tiles can be hidden under carpets.

HSE advises householders not to repair or remove asbestos materials themselves without training. It also says material in good condition is often better left where it is. Tell any builder about it before work starts. Asbestos waste must go to a proper hazardous waste service, and local councils can advise on disposal.